SEGMENTATION OF RADIOGRAPHIC IMAGES OF WELD DEFECT

Wafaa Al-Hameed,Prof. Yahya Mayali and Prof. Phil Picton

The first stage in the classification or identification of defects in gray-level x-ray images of welds is the segmentation of the defects. The gray levels in weld images depend on the density and thickness of the material being tested. This causes the relative contrast of the defect area to vary with its position. As a consequence, it is difficult to carry out the process of segmentation. As a result, the subsequent stages of operations such as classification or recognition are affected. In this paper, different segmentation methods are introduced which are known as “data-driven”. In this approach, only the gray-level data is used to identify an area of interest, i.e. an area of the image that contains a defect, and hence extract it. The comparison of results show that using the morphology process with local thresholding yields better results than using edge detection method such as Sobel and Canny filters.

నిరాకరణ: ఈ సారాంశం ఆర్టిఫిషియల్ ఇంటెలిజెన్స్ టూల్స్ ఉపయోగించి అనువదించబడింది మరియు ఇంకా సమీక్షించబడలేదు లేదా నిర్ధారించబడలేదు

ఇండెక్స్ చేయబడింది

Google Scholar
Academic Journals Database
Open J Gate
Academic Keys
ResearchBible
CiteFactor
ఎలక్ట్రానిక్ జర్నల్స్ లైబ్రరీ
RefSeek
హమ్దార్డ్ విశ్వవిద్యాలయం
విద్వాంసుడు
ఇంటర్నేషనల్ ఇన్నోవేటివ్ జర్నల్ ఇంపాక్ట్ ఫ్యాక్టర్ (IIJIF)
ఇంటర్నేషనల్ ఇన్స్టిట్యూట్ ఆఫ్ ఆర్గనైజ్డ్ రీసెర్చ్ (I2OR)
కాస్మోస్

మరిన్ని చూడండి